MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ravago Manufacturing Americas EZPrene 9040A TPV
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes:

Information provided by Ravago Manufacturing Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  39
@Time 5.00 sec
39
@Time 0.00139 hour
Extruded; ASTM D2240
 41
@Time 5.00 sec
41
@Time 0.00139 hour
Injection Molded; ASTM D2240
Tensile Strength at Break 3.90 MPa566 psiASTM D412
Elongation at Break 555 %555 %ASTM D412
100% Modulus 1.30 MPa
@Strain 100 %
189 psi
@Strain 100 %
ASTM D412
Tear Strength 12.0 kN/m68.5 pliASTM D624
Compression Set  28 %
@Temperature 23.0 °C,
Time 79200 sec
28 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
 38 %
@Temperature 125 °C,
Time 252000 sec
38 %
@Temperature 257 °F,
Time 70.0 hour
ASTM D395B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 130 °C266 °F
Brittleness Temperature -70.0 °C-94.0 °FASTM D746
 
Descriptive Properties
Ozone ResistanceExcellentASTM D1149

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Barlog Plastics KEBAFLEX E 40.1 TPE-V, Shore A40
Chengdu Polyster FR2085 Flame Retardant Grade TPV
ExxonMobil Santoprene® 8191-55B100 Thermoplastic Elastomer
Teknor Apex Sarlink® 3140 Thermoplastic Elastomer
E-Polymers EFLEX® V1040 EPDM/TPV

PRAVAGO2006 / 221956

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.