MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phillips 66 Omniguard® XD5 NLGI Grade 2
Categories: Fluid; Lubricant; Calcium Gellant

Material Notes: Omniguard XD5 is a premium quality, high-performance, extreme pressure (EP) calcium sulfonate grease developed to satisfy the severe lubrication requirements of mining and off-road equipment manufactured by Caterpillar, Terex, Komatsu Dresser, Le Tourneau, P&H and others. It is particularly recommended for use in AC and DC electric-drive haul trucks, cranes, scrapers, shovels and drag lines operating under wet conditions and/or moderate to high temperatures and under heavy loading. Omniguard XD5 is manufactured with high-quality base oils and a non-soap, calcium sulfonate thickener. It is compounded with select additives that provide extreme-pressure and antiwear properties, excellent rust and corrosion protection, and excellent oxidation resistance. It is fortified with 5% molybdenum disulfide(moly) for extra wear protection under heavy or shock loading. Functional polymers provide better adhesion to metal surfaces and enhanced resistance to water washout in wet environments.

Applications:

  • Chassis parts and wheel bearings of mine haul trucks and other off-highway equipment
  • Heavily loaded plain and rolling-element bearings in industrial and mobile equipment where the manufacturer specifies a high-temperature, extreme-pressure grease with 5% moly
Features/Benefit:
  • High dropping point (>550°F)
  • High load-carrying capacity
  • Excellent wear protection
  • Contains 5% moly for extra protection against galling and wear under shock loads
  • Excellent oxidation resistance
  • Excellent resistance to water washout
  • Excellent rust and corrosion protection

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.29 lb/gal
Viscosity Measurement 44Index
Saybolt Viscosity at 100°F 803 SUS
Saybolt Viscosity at 210°F 66 SUS
Kinematic Viscosity at 40°C (104°F) 150 cSt
Kinematic Viscosity at 100°C (212°F) 11.5 cSt
Oxidative Stability 100 hour
@Pressure 0.0207 MPa
Pressure Drop; ASTM D942
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 800 kgASTM D2596
Four Ball Wear <= 0.500 mmScar Diameter; ASTM D2266
Penetration 265 - 295
Timken Test 60.0 lbOK Load; ASTM D2509
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °C
Minimum Service Temperature, Air -29.0 °C
Dropping Point >= 288 °C
 
Descriptive Properties
ColorGray-Black
Composition5%Molybdenum Disulfide
ThickenerCalcium Sulfonate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5137 / 198390

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.