MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Mindel® B-430 Polysulfone, Modified (PSU, Modified)  (discontinued **)
Categories: Polymer; Thermoplastic; Polysulfone (PSU); Polysulfone, 30% Glass Fiber Reinforced

Material Notes: Mindel B-430 is a 30% glass reinforced thermoplastic with excellent dimensional stability, exceptional resistance to warp, good chemical resistance, and high stiffness. It was developed specifically for electrical/electronic applications requiring flame resistance, but where flame retardant systems based on polybrominated diphenyl- oxides or ethers are undesirable. The resin has a UL 94 V0 rating at 0.062" (1.57 mm) thickness, even though it does not contain polybrominated diphenyl- ethers or oxides. This material can therefore be used in areas of the world where the use of flame retardants based on polybrominated diphenylethers/ oxides may be restricted. Mindel B-430 resin's resistance to warping results from low isotropic shrinkage. Combined with high stiffness, good creep resistance and high heat distortion temperature, Mindel B-430 resin may be ideally suited for use in demanding electrical components such as relays, switches, motor starters and control housings. Mindel B-430 resin should also be considered for electrical connectors that do not have the demanding temperature requirements of surface mount technology. The material has excellent regrind stability and, unlike polyesters, retains a high level of mechanical and electrical properties even at elevated temperatures and humidities. - Black: Mindel B-430 BK 174 - Natural: Mindel B-430 NT - Grey: Mindel B-430 GY 674 - Custom Colorable

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.52 g/ccASTM D792
Filler Content 30 %Glass Fiber
Water Absorption 0.10 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0025 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cmASTM D955
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 275 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 121 MPaASTM D638
Elongation at Break 2.5 %ASTM D638
Flexural Strength 185 MPaASTM D790
Flexural Modulus 9380 MPaASTM D790
Izod Impact, Notched 96.1 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmASTM D257
Comparative Tracking Index 180 VUL 746
 175 - 250 VPLC 3; UL 746
Hot Wire Ignition, HWI 120 secUL 746
 >= 120 secPLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR 10.0 mm/minUL 746
 <= 10.0 mm/minPLC 0; UL 746
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 166 °CUnannealed; ASTM D648
UL RTI, Electrical 150 °CUL 746
UL RTI, Mechanical with Impact 150 °CUL 746
UL RTI, Mechanical without Impact 150 °CUL 746
Flammability, UL94 V-0
@Thickness 1.57 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 271 - 288 °C
Drying Temperature 135 - 163 °C
@Time 10800 - 14400 sec
Injection Pressure 103 - 138 MPa
 
Descriptive Properties
AdditiveFlame Retardant
AppearanceColors Available
 Natural Color
AvailabilityAsia Pacific
 Europe
 North America
 South America
FeaturesFlame Retardant
 Good Chemical Resistance
 Good Creep Resistance
 Good Dimensional Stability
 High Stiffness
 Warp Resistant
FormsPellets
Processing MethodInjection Molding
RoHS ComplianceRoHS Compliant
UsesAppliance Components
 Appliances
 Business Equipment
 Electrical Housing
 Electrical Parts
 Electrical/Electronic Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 1000-2 NF2001 PA66 (Dry)
Celanese Celanex® 2016 PBT, Unfilled
Syensqo (Solvay Specialty Polymers) Mindel® S-1000 Modified Polysulfone
Syensqo (Solvay Specialty Polymers) Mindel® B-322 Polysulfone, Modified (PSU, Modified)
Mitsubishi Iupilon® MB4306R PC/Polyester

PSOL8Y922 / 107706

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.