MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI 4620 Steel, normalized, machined to 13.7 mm rounds, pseudocarburized, reheated to 775°C (1430°F), quenched and tempered
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel; Low Alloy Steel; Carbon Steel; Low Carbon Steel

Material Notes: Normalized at 925°C (1700°F) in 32 mm rounds, machined to 13.7 mm rounds, pseudocarburized at 925°C (1700°F) for 8hrs., box cooled to RT, reheated to 775°C (1430°F), oil quenched, 150°C (300°F) temper. Tested in 12.8 mm rounds.

Key Words: SAE J404, SAE J412, SAE J791, UNS G46200, AMS 6294, ASTM A322, ASTM A331, ASTM A505, ASTM A535, MIL SPEC MIL-S-7493 (A4620)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 277
Hardness, Knoop 302Converted from Brinell
Hardness, Rockwell B 99Converted from Brinell
Hardness, Rockwell C 28Converted from Brinell
Hardness, Vickers 292Converted from Brinell
Tensile Strength, Ultimate 910 MPa
Tensile Strength, Yield 738 MPa
Elongation at Break 14 %in 50 mm
Reduction of Area 48 %
Modulus of Elasticity 205 GPaTypical for steel
Bulk Modulus 160 GPaTypical for steel
Poissons Ratio 0.29Calculated
Machinability 65 %Hot rolled and cold drawn. Based on 100% machinability for AISI 1212 steel.
Shear Modulus 80.0 GPaTypical for steel
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000245 ohm-cmTypical 4000 series steel
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.475 J/g-°CTypical 4000 series steel
Thermal Conductivity 44.5 W/m-KTypical steel
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.17 - 0.22 %
Iron, Fe 96.405 - 97.38 %As remainder
Manganese, Mn 0.45 - 0.65 %
Molybdenum, Mo 0.20 - 0.30 %
Nickel, Ni 1.65 - 2.0 %
Phosphorus, P <= 0.035 %
Silicon, Si 0.15 - 0.35 %
Sulfur, S <= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI 4620 Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, reheated to 775°C (1430°F), quenched and tempered
AISI 4620 Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, reheated to 925°C (1700°F), quenched and tempered
AISI 4620 Steel, quenched 900°C (1650°F), 425°C (800°F) temper
AISI 4620 Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, reheated to 800°C (1470°F), quenched and tempered
AISI 4620 Steel, normalized, machined to 25 mm (1 in.) rounds, pseudocarburized, reheated to 830°C (1525°F), quenched and tempered

M462AV / 7893

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.