MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake EMAC® SP 1257 Ethylene-Methyl Acrylate Copolymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Film Grade

Material Notes: 20% Methyl Acrylate Content. Characteristics: FDA Clearance for Packaging of Most Foods, Including Aseptic Packaging; Less Crystalline and Softer than Polyethylene; Excellent Heat Stability Allows Processing Temperature Range of 280-600°F; Non-corrosive at all Temperature Ranges; No FDA Thickness Limitations; Contains a High Level of Slip and Antiblock Additives

Applications:Film: Excellent Heat Seal Response at Low Temperatures, Making it a Good Candidate for the Heat Seal Layer in Various Coextrusion Constructions; Coatings & Laminations: Higher Neck-In but Similar Drawdown vs. Polyethylene, Excellent Heat Seal Response at Low Seal Temperatures, Processing Temperature Range - 580-600°F, Can be Drawn as Low as 4 lbs. per ream, Gas Barrier and Grease Resistance are Slightly Less than those of LDPE; Coextrusion: Excellent Coextrusion Tie Layer for LDPE, LLDPE, HDPE, PP, EVA, EEA, Ionomer, PET, PC, PVDC and rigid PVC; Injection Molding: Processing Temperature 360-600°F, Less Mold Shrinkage than LDPE, Produces Very Tough, Stress Crack Resistant Parts

Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no longer appears in the Westlake product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.944 g/ccASTM D1505
ESCR 10% Igepal® >= 360 hour
@Temperature 50.0 °C
F50; ASTM D1693
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Cond. E; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90ASTM D2240
Hardness, Shore D 31ASTM D2240
Tensile Strength, Ultimate 11.4 MPaASTM D638
Elongation at Break 750 %ASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 82.0 °Cby DSC
Vicat Softening Point 58.0 °CASTM D1525
Brittleness Temperature <= -76.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 154 °CBlown Film
 190 °CMolding
 315 °CExtrusion Coating

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade
Arkema LOTRYL® Bestpeel 2407 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 29 MA 03 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 28 MA 07 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 24 MA 005 Copolymer Ethylene - Methyl Acrylate

PCHEVVB8 / 20514

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.