MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber
Categories: Polymer; Thermoplastic; Polyetherimide (PEI); Polyetherimide (PEI), 10% Glass Fiber

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 10% Glass Fiber". Specific grades with glass content between 5% and 14% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Ensinger TECAPEI™ glass fiber reinforced shapes, made from ULTEM® PEI with Ensinger's proprietary extrusion techniques, provide superior tensile strength, rigidity, and dimensional stability for your most demanding PEI applications.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.30 - 1.90 g/ccAverage value: 1.49 g/cc Grade Count:24
Filler Content 5.00 - 50.0 %Average value: 29.7 % Grade Count:14
Water Absorption 0.210 - 0.270 %Average value: 0.232 % Grade Count:12
Linear Mold Shrinkage 0.000500 - 0.00700 cm/cmAverage value: 0.00496 cm/cm Grade Count:15
Melt Flow 5.00 - 22.0 g/10 minAverage value: 8.93 g/10 min Grade Count:3
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 114 - 121Average value: 118 Grade Count:4
Tensile Strength, Ultimate 68.9 - 450 MPaAverage value: 210 MPa Grade Count:21
Tensile Strength, Yield 110 - 121 MPaAverage value: 115 MPa Grade Count:5
Elongation at Break 1.00 - 11.0 %Average value: 4.85 % Grade Count:16
Modulus of Elasticity 4.48 - 24.0 GPaAverage value: 12.0 GPa Grade Count:17
Flexural Yield Strength 124 - 570 MPaAverage value: 289 MPa Grade Count:22
Flexural Modulus 2.60 - 26.0 GPaAverage value: 10.1 GPa Grade Count:24
Compressive Yield Strength 152 - 670 MPaAverage value: 497 MPa Grade Count:9
Compressive Modulus 3.73 - 27.0 GPaAverage value: 23.7 GPa Grade Count:7
Izod Impact, Notched 0.320 - 4.27 J/cmAverage value: 0.730 J/cm Grade Count:18
Izod Impact, Unnotched 2.14 - 12.8 J/cmAverage value: 6.01 J/cm Grade Count:11
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1000 - 1.00e+17 ohm-cmAverage value: 3.09e+16 ohm-cm Grade Count:11
Dielectric Constant 3.50 - 3.60Average value: 3.54 Grade Count:5
Dielectric Strength 19.7 - 27.6 kV/mmAverage value: 23.0 kV/mm Grade Count:7
Dissipation Factor 0.00140 - 0.00500Average value: 0.00313 Grade Count:5
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 - 54.0 µm/m-°CAverage value: 26.2 µm/m-°C Grade Count:15
Thermal Conductivity 0.176 - 0.231 W/m-KAverage value: 0.213 W/m-K Grade Count:4
Maximum Service Temperature, Air 171 - 200 °CAverage value: 188 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 196 - 223 °CAverage value: 210 °C Grade Count:13
Deflection Temperature at 1.8 MPa (264 psi) 189 - 221 °CAverage value: 206 °C Grade Count:17
Vicat Softening Point 221 - 223 °CAverage value: 222 °C Grade Count:3
Glass Transition Temp, Tg 217 °CAverage value: 217 °C Grade Count:6
Flammability, UL94 V-0 - 5VAGrade Count:10
 
Processing PropertiesOriginal ValueComments
Processing Temperature 349 - 382 °CAverage value: 368 °C Grade Count:6
Melt Temperature 332 - 399 °CAverage value: 366 °C Grade Count:7
Mold Temperature 107 - 177 °CAverage value: 152 °C Grade Count:12
Drying Temperature 143 - 152 °CAverage value: 149 °C Grade Count:13
Moisture Content 0.0200 - 0.0400 %Average value: 0.0320 % Grade Count:5
Dew Point -28.9 °CAverage value: -28.9 °C Grade Count:3
Injection Pressure 82.7 - 124 MPaAverage value: 103 MPa Grade Count:8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
Overview of materials for Polyetherimide (PEI)

O3611 / 78225

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.