MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beryllium Copper, UNS C17300, TD01 Temper Strip
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot formability. Commonly fabricated by blanking, forming and bending, turning, drilling, tapping.

Applications: springs, flexible metal hose, Bourdon tubing, bellows, clips, washers, retaining rings, and other parts subject to severe forming conditions but require high strength, anelasticity, and fatigue and creep resistance; in parts that require high strength or wear resistance along with good electrical conductivity and/or magnetic characteristics such as navigational instruments, non-sparking safety tools, firing pins, bushings, valves, pumps, shafts, and rolling mill parts.

Proprietary mill treatment to produce the indicated tensile properties.

Key Words: BeCu; CDA 173, ISO CuBe2Pb, CEN CW102C; Alloy M25
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.25 g/ccduring age hardening, 2% max. decrease in length and 6% max. increase in density.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 68 - 90
Hardness, Rockwell C >= 36
Hardness, Rockwell 30T 62 - 75
Hardness, Vickers 150 - 190
Tensile Strength, Ultimate 515 - 605 MPa
Tensile Strength, Yield 415 - 605 MPa
@Strain 0.2 %
Elongation at Break 10 - 36 %in 50 mm
Modulus of Elasticity 125 - 130 GPa
Poissons Ratio 0.30
Fatigue Strength 215 - 250 MPa
@# of Cycles 1.00e+8
Reverse Bending
Machinability 50 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 50.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000096 - 0.000011 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.7 µm/m-°C
@Temperature 20.0 - 100 °C
 17.0 µm/m-°C
@Temperature 20.0 - 200 °C
 17.8 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.420 J/g-°C
Thermal Conductivity 105 - 130 W/m-K
@Temperature 20.0 °C
 130 - 133 W/m-K
@Temperature 200 °C
Melting Point 865 - 980 °C
Solidus 865 °C
Liquidus 980 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 845 °CHot-Shortness Temperature
Annealing Temperature 760 - 790 °C
Solution Temperature 760 - 790 °C
Aging Temperature 260 - 425 °C
Hot-Working Temperature 650 - 800 °C
Precipitation Temperature 600 °F
@Time 180 sec
Air
Recrystallization Temperature 730 °C
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 1.8 - 2.0 %
Co + Ni >= 0.20 %
Co + Ni + Fe <= 0.60 %
Copper, Cu 97 %
Lead, Pb 0.20 - 0.60 %
Other, total <= 0.50 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Beryllium Copper, UNS C17300, TB00 Temper Strip
Beryllium Copper, UNS C17300, TF00 Temper Strip
Beryllium Copper, UNS C17200, TB00 Temper Strip
Beryllium Copper, UNS C17000
Beryllium Copper, UNS C17200, TD04 Temper Strip

MC17300b2 / 10817

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.