MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M 7660-S-HSG Cold Shrink QT-III Silicone Rubber Skirted Termination Kits
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: 3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7650-S-HSG and 7660-S-HSG Series, are designed for applications requiring a high-ampacity ground. Each kit contains one-piece, skirted, silicone rubber termination with high-ampacity ground assembly and is qualified as IEEE Standard 48 Class 1 for outdoor weather-exposed applications. The termination assemblies consist of a skirted insulator, high-dielectric constant (High-K) stress control tube, conformable High-K stress controlling compound and built-in environmental top sealing compound. The insulator is made of a dark gray silicone rubber with excellent tracking resistance and hydrophobic properties.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 10.3 MPaHigh-K Stress Control Tube; ASTM D412
100% Modulus 0.00110 GPa
@Strain 100 %
High-K Stress Control Tube; ASTM D412
300% Modulus 0.500 ksi
@Strain 300 %
High-K Stress Control Tube; ASTM D412
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 22
@Frequency 60.0 Hz
High-K Stress Control Tube, 1000 V, 50% RH; ASTM D150
 25
@Frequency 60.0 Hz
High-K Stress Control Compound, 1000 V, 50% RH, 100 mil; ASTM D150
Dielectric Strength 300 kV/in
@Thickness 1.91 mm
Environmental Sealing Compound; ASTM D149
Dissipation Factor 0.10
@Frequency 60 Hz
High-K Stress Control Tube, 1000 V, 50% RH; ASTM D150
 0.90
@Thickness 2.54 mm,
Frequency 60 Hz
High-K Stress Control Compound, 1000 V, 50% RH; ASTM D150

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek TS-107 Thermoset Electrical Insulation Product (Nema Grade: G-7)
Plenco 6401 Phenolic, Briquette, Injection Molded
Overview of materials for Silicone Rubber
Overview of materials for Polyetherimide (PEI)
Master Bond EP121AO Thermally Conductive, Dimensionally Stable Epoxy System

PMM35155 / 169902

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.