MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Adflex C 200F Thermoplastic Polyolefin
Categories: Polymer; Film; Thermoplastic; Polyolefin

Material Notes: Adflex C 200 F is developed for the central layer of tough, transparent co-extruded cast-film structures. It combines transparency with high softness , a very high toughness even at low temperatures and an excellent compatibility with other polyolefins. It does not contain any slip nor anti-blocking agents. Typical applications of the Adflex C 200 F are co-extruded cast-film for food packaging, hygiene applications, surface protection where the outside layer can be any polyolefin homo or copolymer. Applications: Bags & Pouches, Barrier Film, Breathable Film, Film Wrap, Food Packaging Film, Lamination Film, Peelable Film, Stationery Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccMethod A; ISO 1183-1
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 41ISO 868
Film Tensile Strength at Yield, MD 8.00 MPa
@Thickness 0.0500 mm
500 mm/min; ISO 527-3
Film Tensile Strength at Yield, TD 8.00 MPa
@Thickness 0.0500 mm
500 mm/min; ISO 527-3
Tensile Strength, Yield 8.00 MPaISO 527-1,-2
Film Elongation at Break, MD 990 %
@Thickness 0.0500 mm
500 mm/min; ISO 527-3
Film Elongation at Break, TD 890 %
@Thickness 0.0500 mm
500 mm/min; ISO 527-3
Film Elongation at Yield, MD 26 %
@Thickness 0.0500 mm
500 mm/min; ISO 527-3
Film Elongation at Yield, TD 23 %
@Thickness 0.0500 mm
500 mm/min; ISO 527-3
Elongation at Break 500 %ISO 527-1,-2
Flexural Modulus 220 MPaISO 178
Secant Modulus, MD 0.125 GPa23 mm/min, cast film; ISO 527-3
Secant Modulus, TD 0.110 GPa23 mm/min, cast film; ISO 527-3
Izod Impact, Notched (ISO) 65.0 kJ/m²
@Temperature -20.0 °C
Type 1, Notch A; ISO 180
 NB
@Temperature 23.0 °C
Type 1, Notch A; ISO 180
Film Tensile Strength at Break, MD 30.0 MPa
@Thickness 0.0500 mm
500 mm/min; ISO 527-3
Film Tensile Strength at Break, TD 24.0 MPa
@Thickness 0.0500 mm
500 mm/min; ISO 527-3
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 89.0 °CA50, 50°C/h, 10N; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 8.0 %
@Thickness 0.0500 mm
ASTM D1003
Gloss 47 %
@Thickness 0.0500 mm
@ 45°; ASTM D 2457
 
Descriptive Properties
Processing MethodCast Film, Extrusion Coating, Extrusion Thermoforming.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Adflex Q 300F Thermoplastic Polyolefin
LyondellBasell Adflex 7637 XCP Thermoplastic Polyolefin
LyondellBasell Adflex 7634 XCP Thermoplastic Polyolefin

PEQT7011 / 218650

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.