MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Alliance Polymers Viprene™ P90A-22U-NAT Thermoplastic Vulcanizate Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Viprene™ P90A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing characteristics.

Availability: North America

Additive: Heat Stabilizer and UV Stabilizer

Features: Good Flow, Good UV Resistance and Heat Stabilized

Appearance: Natural Color

Forms: Pellets

Processing Method: Extrusion and Injection Molding

Information provided by Alliance Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccISO 2781
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90ISO 868
Hardness, Shore D 38ISO 868
Tensile Strength at Break 1900 psiISO 37
Tensile Stress at Strain 1100 psi
@Strain 100 %
ISO 37
 1460 psi
@Strain 300 %
ISO 37
Elongation at Break 500 %ISO 37
Tear Strength 360 pliISO 34-1
Compression Set 35 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D3995B
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -76.0 °FASTM D746
Flammability, UL94 HB
@Thickness 1.00 mm
 HB
@Thickness 1.50 mm
 HB
@Thickness 3.00 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 205 °CGate Temperature; Extrusion
 392 - 446 °FInjection
Rear Barrel Temperature 356 °FInjection
Middle Barrel Temperature 374 °FInjection
Front Barrel Temperature 383 °FInjection
Nozzle Temperature 383 - 437 °FInjection
Zone 1 365 °FExtrusion
Zone 2 383 °FExtrusion
Zone 3 392 °FExtrusion
Die Temperature 410 °F
@Pressure 4.80 - 17.0 MPa
Extrusion
Mold Temperature 50.0 - 122 °FInjection
Injection Velocity >= 50.0 mm/secInjection
Drying Temperature 176 °FInjection
 176 °FExtrusion
Dry Time 3.00 hourInjection
 3.00 hourExtrusion
Back Pressure 58.0 - 116 psiInjection
Clamp Pressure 5800 - 10200 psiInjection
Screw Speed 100 - 200 rpmInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Barlog Plastics KEBAFLEX E 35.1 TPE-V, Shore A35
ExxonMobil Santoprene® 8211-25 Thermoplastic Elastomer
DSM Biomedical CarboSil® 40 90A Biocompatible Silicone Polycarbonate Urethane
DSM Biomedical CarboSil® 10 90A Biocompatible Silicone Polycarbonate Urethane
Celanese SO.F.TER Forprene® 6NM.A80 TPE

PAPS050 / 159423

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.