MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celstran® PP-GF40-04 PP, 40% Glass Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Glass Fiber Filler

Material Notes: Material code according to ISO 1043-1: PP
PP-GF with 40 % chemically coupled long glas fibers

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPa5mm/min; ISO 527-2/1A
Tensile Strength 63.0 MPa
@Temperature 80.0 °C
ISO 527-1, -2
Elongation at Break 2.0 %5mm/min; ISO 527-2/1A
 2.5 %
@Temperature 80.0 °C
ISO 527-1, -2
Tensile Modulus 9100 MPa1mm/min; ISO 527-2/1A
 6500 MPa
@Temperature 80.0 °C
ISO 527-1, -2
Flexural Strength 190 MPaISO 178
 100 MPa
@Temperature 80.0 °C
ISO 178
Flexural Modulus 9500 MPaISO 178
 6400 MPa
@Temperature 80.0 °C
ISO 178
Charpy Impact Unnotched 59.0 kJ/m²ISO 179/1eU
 55.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 16.0 kJ/m²ISO 179/1eA
 13.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 162 °C10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 152 °CISO 75-1, -2
Deflection Temperature at 8.0 MPa 128 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 70.0 °CCavity temperature
Feed Temperature 20.0 - 50.0 °C
Zone 1 250 - 260 °C
Zone 2 260 - 270 °C
Zone 3 270 - 280 °C
Zone 4 280 - 290 °C
Die Temperature 260 - 290 °C
Melt Temperature 270 °CInjection molding; ISO 294
 260 - 290 °Cin the screw anteroom
Mold Temperature 40.0 - 70.0 °C
 70.0 °CInjection molding; ISO 294
Injection Velocity 80.0 mm/secISO 294
Drying Temperature 90.0 - 100 °C
Dry Time 4.00 hour
Moisture Content 0.20 %Necessary low maximum residual
Injection Pressure 60.0 - 120 MPa
Hold Pressure 40.0 - 80.0 MPa
 83.0 MPaISO 294
Back Pressure 3.00 MPa
Screw Speed 25 rpm
@Diameter 75.0 mm
 35 rpm
@Diameter 55.0 mm
 50 rpm
@Diameter 40.0 mm
Hot-Working Temperature 260 - 290 °C
 
Descriptive Properties
Heat stabilized/stable to heatYes
Injection moldingYes
Injection speedslow
Longer pre-drying times/storageCan be stored in standard conditions until processed.
Pre-dryingDrying is not normally required with proper storage
Sheet extrusionYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celstran® +PP-GF40-04CN03 PP, 40% Glass Reinforced
Celanese Celstran® PP-GF40-03 PP, 40% Glass Reinforced
Celanese Celstran® PP-GF40-03-Black PP, 40% Glass Reinforced
Celanese Celstran® PP-GF40-0414P10/10 PP, 40% Glass Reinforced
Celanese Celstran® PP-GF50-0453P10/10 PP, 50% Glass Reinforced

PHCR200 / 158769

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.