MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil EXACT™ 3027 Plastomer for Cast Film Applications
Categories: Polymer; Film; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO), Film Grade; Polyethylene (PE)

Material Notes: Product Description: Exact 3027 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 3027 is designed for both monolayer and multilayer coextruded cast film applicatiosn requiring excellent toughness and heat sealing performance. Typical applicatiosn include seal layers for meat, poultry, and cheese packaging, lamination films, heavy duty bags, and cereal box liner packaging.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Cast Film
  • Heavy Duty Bags
  • Lamination Film

Data provided by the manufacturer, Exxon Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccExxon Method
Thickness 0.800 mil
Melt Flow 3.5 g/10 minExxon Method
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 6.27 MPaASTM D882
Film Tensile Strength at Yield, TD 4.30 MPaASTM D882
Film Elongation at Break, MD 490 %ASTM D882
Film Elongation at Break, TD 810 %ASTM D882
Film Elongation at Yield, MD 10 %ASTM D882
Film Elongation at Yield, TD 8.0 %ASTM D882
Secant Modulus, MD 0.0669 GPa1% secant; ASTM D882
Secant Modulus, TD 0.0758 GPa1% secant; ASTM D882
Puncture Energy 57.0 in-lbExxon Method
Elmendorf Tear Strength, MD 180 g/milASTM D1922
Elmendorf Tear Strength, TD 250 g/milASTM D1922
Dart Drop 230 g/milASTM D1709
Film Tensile Strength at Break, MD 58.0 MPaASTM D882
Film Tensile Strength at Break, TD 35.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 90.0 °CExxon Method
 
Optical PropertiesOriginal ValueComments
Haze 0.40 %ASTM D1003
Gloss 94 %45°; ASTM D-2457
 
Descriptive Properties
Puncture Force14 lbfExxon Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Cogegum® AFR/710 Polyolefin
ExxonMobil LDPE LD 363BW Low Density Polyethylene Resin
ExxonMobil LDPE LD 319.92 Low Density Polyethylene Resin
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin (Asia Pacific Grade)

PEXCI3 / 38023

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.