MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient OnFlex™ S EF 50A-3S1965 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excellent processability, in addition to typical OnFlex™-S properties such as a wide hardness range, low compression set, good colourability and a wide temperature operating range. OnFlex™-S EF compounds are semi-filled, making them opaque and with a medium density.

Properties are measured using injection molded plaques.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050ISO 868
Tensile Strength at Break 6.30 MPa914 psiISO 37
Tensile Stress at Strain  1.50 MPa
@Strain 100 %
218 psi
@Strain 100 %
ISO 37
 2.30 MPa
@Strain 300 %
334 psi
@Strain 300 %
ISO 37
Elongation at Break 680 %680 %ISO 37
Tear Strength 25.0 kN/m143 pliISO 34-1
Compression Set  15 %
@Temperature 23.0 °C,
Time 259000 sec
15 %
@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
 63 %
@Temperature 70.0 °C,
Time 79200 sec
63 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 95 %
@Temperature 100 °C,
Time 79200 sec
95 %
@Temperature 212 °F,
Time 22.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 220 °C356 - 428 °F
Mold Temperature 30.0 - 60.0 °C86.0 - 140 °F
 
Descriptive Properties
FeaturesHigh Flow
FormsPellets
Generic MaterialTPE
Generic Material TypeStyrenic Thermoplastic Elastomer (TES)
Generic NameThermoplastic Elastomer (TPE)
Injection RateFast
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesAppliances
 Automotive Applications
 Consumer Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Propylene Oxide Rubber (GPO)
Dow S40 LIQUID SILICONE RUBBER KIT
Covestro Bayflex® 952 Polyether-based Polyurethane System, Density 34 pcf

PH0POL1138 / 145707

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.