MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Special Metals NIMONIC® Alloy 263
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: A precipitation-hardenable nickel-chromium-cobalt alloy with an addition of molybdenum for solid-solution strengthening. It has high strength and corrosion resistance along with good formability and high-temperature ductility in welded structures. The alloy is especially suitable for sheet applications. Used in gas turbines for rings, casings, and various sheet fabrications. Standard product forms are round, flats, extruded section, tube, plate, sheet, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: Nickel-Chromium Alloy; Werkstoff Nr. 2.4650, UNS N07263; BS HR10, HR206, HR404; SAE AMS 5872; WL Nr. 2.4650; AFNOR NCK 20D; AECMA Pr EN 2199-2203, 2418
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.36 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 760 MPa
@Temperature 650 °C
Precipitation Hardened prior to test
 940 MPa
@Temperature 23.0 °C
Tensile Strength, Yield 550 MPa
@Strain 0.2 %
Precipitation Hardened. Value at room temperature
 450 MPa
@Strain 0.2 %,
Temperature 650 °C
Precipitation Hardened prior to test
Elongation at Break 39 %Precipitation Hardened
 30 %
@Temperature 650 °C
Precipitation Hardened prior to test.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000115 ohm-cm
Magnetic Permeability 1.0008at 200 Oersted (15.9 kA/m)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.3 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.461 J/g-°C
Thermal Conductivity 11.7 W/m-K
Melting Point 1300 - 1355 °C
Solidus 1300 °C
Liquidus 1355 °C
 
Component Elements PropertiesOriginal ValueComments
Al + Ti 2.4 - 2.8 %
Aluminum, Al <= 0.60 %
Boron, B <= 0.0050 %
Carbon, C 0.040 - 0.080 %
Chromium, Cr 19 - 21 %
Cobalt, Co 19 - 21 %
Copper, Cu <= 0.20 %
Iron, Fe <= 0.70 %
Manganese, Mn <= 0.60 %
Molybdenum, Mo 5.6 - 6.1 %
Nickel, Ni 49 %As remainder
Silicon, Si <= 0.40 %
Sulfur, S <= 0.0070 %
Titanium, Ti 1.9 - 2.4 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® Nickelvac® C-263 Nickel Superalloy, Heat Treatment: 927°C (1700°F) Anneal
Special Metals INCONEL® Alloy 625
Special Metals NIMONIC® Alloy 80A
Special Metals NIMONIC® Alloy 90
Special Metals NIMONIC® Alloy 75

NINC67 / 17417

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.