MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Elastosil® LR 3070/60 A/B Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Self-adhesive liquid silicone rubbers of the ELASTOSIL® LR 3070 series are paste-like, easily pigmentable two-component compounds with extremely short curing times.

ELASTOSIL® LR 3070 series are primerless, selfbonding grades that adhere to various plastic substrates (e. g. PA, PBT) and metals, but not in the mold. The bonding is improved by an ageing-process (e. g. one hour at 100°C) or by a longer storing at room temperature. Because of the individual surface properties each substrate must be tested before mass production. The vulcanizates are noted for good mechanical and electrical properties.

Application: ELASTOSIL® LR 3070 series are particularly suitable for the economical production of large series of overmolded parts (thermoplastic/elastomer), even in a comolding process (shuttle mold) under standard conditions, without any special treatment of the mold surface. Parts made from ELASTOSIL® LR 3070 can generally be used for technical applications without post-curing, but do not comply with regulations concerning use in the pharmaceutical and food industry.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccISO 1183-1 A
Viscosity 350000 cP
@Shear Rate 10.0 1/s
DIN 53019
 1.10e+6 cP
@Shear Rate 0.900 1/s
DIN 53019
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 57DIN 53505
Tensile Strength at Break 7.70 MPaDIN 53504 S 1
Elongation at Break 420 %DIN 53504 S 1
Tear Strength 23.0 kN/mASTM 624 B
Compression Set 16 %
@Temperature 125 °C,
Time 79200 sec
DIN ISO 815-B
 32 %
@Temperature 150 °C,
Time 79200 sec
DIN ISO 815-B
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 210 °Cwith heat stabilizer
Minimum Service Temperature, Air -55.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %"Transparent" but manufacturer does not quantify.
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Treatment Temp. 165 °C
in press
 
Descriptive Properties
Appearancetransparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Elastosil® LR 3072/50 A/B Liquid Silicone Rubber

PWACK9137 / 204666

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.