MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Wacker® Methyl acetate 99.5%
Categories: Fluid

Material Notes: Empirical formula: C3H6O2

CAS No.: 79-20-9

Product description: WACKER® Methyl Acetate 99,5 % is a clear, colorless, neutral liquid with a mild, ester-like odor. Methyl acetate is one of the best solvents available. It is used predominantly for dyes and in the coatings, adhesives, cosmetics, plant-protection and pharmaceutical industries.

Application:

  • parquet Adhesives
  • all Purpose Adhesives
  • interior Paints
  • solvent for chemical Industries

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.933 g/cc
Vapor Pressure 0.217 atm
@Temperature 20.0 °C
 0.771 atm
@Temperature 50.0 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point -98.0 °C
Boiling Point 55.0 - 57.0 °C
@Pressure 0.1013 MPa
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.361 - 1.363
Transmission, Visible 90 %"Clear" but manufacturer does not quantify.
 
Descriptive Properties
Appearanceclear
Color<10 Hazen
Content<100 ppmAcetaldehyde
 <35 ppmAcetic acid
 <500 ppmWater, DIN 51777
 <900 ppmMethanol
Content (%)0.01Acetone
 0.05C12-Isoparaffins
 0.2Acetaldehyde dimethylacetal
Solubility239 g/lin water

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9792 / 205321

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.