MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NRI Syntho-Glass® 24 Fiberglass Mat
Categories: Ceramic; Glass; Glass Fiber

Material Notes: Description: Syntho-Glass®24 consists of a thick fiberglass mat which is pre-impregnated with a water activated resin that hardens into a high energy absorbing and impact resistant rock shield. This system, when used with the preapproved corrosion coating of your choice, provides exceptional mechanical and impact protection on steel, galvanized, concrete, FRP, iron, PVC, and wood. Syntho-Glass 24 can be used underwater, underground or above ground pipes and piles.

Typical Applications:

  • Mechanical protection
Benefits:
  • Impact resistance
  • Energy absorbing
  • Easy to apply
  • No mixing, no measuring ensures consistent glass to resin ratio, therefore consistent results
  • Can be applied in any weather condition, even underwater
  • Our thickest water activated fiberglass provides strong impact resistant shell with only 4 layers
  • Contains no solvents

Information provided by NRI® Innovative Composite Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 309 MPaASTM D3039
Tensile Modulus 20.0 GPaASTM D3039
Impact Test 167 JASTM G14/G62
 
Electrical PropertiesOriginal ValueComments
Dielectric Breakdown 16060 VASTM D149
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °C
Minimum Service Temperature, Air -46.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 hourSet Time, with fast cure resin
 2.00 hourSet Time
Working Life 5.00 minWorking time, fast cure resin
 30.0 min
Shelf Life 6.00 Month
 24.0 Monthfast cure resin

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fiberglass Grade B
NRI Syntho-Glass® Fiberglass
Isoflon Tisoflon® 3 AD Polytetrafluoroethylene Coated Glass Fabric
Isoflon Tisoflon® 6 AD EXTRA SMOOTH Polytetrafluoroethylene Coated Glass Fabric
NRI Solar-Wrap Fiberglass wrap

PNRI010 / 192026

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.