MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ASTM class 35 Standard gray iron test bars, as cast
Categories: Metal; Ferrous Metal; Cast Iron; Gray Cast Iron

Material Notes: 1293 kg transverse load on test bar.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.15 g/ccTypical for Gray Cast Iron
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 212
Hardness, Knoop 236Converted from Brinell
Hardness, Rockwell C 13.7Approximated. Converted from Brinell hardness. Value below normal HRC range, for comparison purposes only.
Hardness, Vickers 223Approximated. Converted from Brinell hardness.
Tensile Strength, Ultimate 252 MPa
Modulus of Elasticity 100 - 119 GPa
Ultimate Compressive Strength 855 MPa
Poissons Ratio 0.29Calculated
Fatigue Strength 110 MPaReversed bending fatigue limit
Shear Modulus 40.0 - 48.0 GPa
Shear Strength 334 MPaTorsional shear strength.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 3.25 - 3.5 %
Chromium, Cr 0.050 - 0.45 %
Copper, Cu 0.15 - 0.40 %
Iron, Fe 91.9 - 94.2 %As Balance
Manganese, Mn 0.50 - 0.90 %
Molybdenum, Mo 0.050 - 0.10 %
Nickel, Ni 0.050 - 0.20 %
Phosphorus, P <= 0.12 %
Silicon, Si 1.8 - 2.3 %
Sulfur, S <= 0.15 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM class 30 Standard gray iron test bars, as cast
Gray Cast Iron, ASTM A 48 Class 40
ASTM class 40 Standard gray iron test bars, as cast
ASTM class 20 Standard gray iron test bars, as cast
ASTM class 25 Standard gray iron test bars, as cast

MCFE13 / 10407

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.