MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
JSC Agidol-1 technical
Categories: Other Engineering Material

Material Notes: Agidol-1 technical (Butylated hydroxytoluene (BHT); 4-methyl-2,6-di-tert-butylphenol; 2,6-di-tert-butyl-paracresol)

Description: Agidol-1 technical is intended for use as an antioxidant additive, it is an efficient stabilizer for wide range of polymeric materials, various rubbers. It is a heat stabilizer for polyolefines, polystyrene, thermoplastic glue and coatings, it protects lubricating and transformation oils, petrol, different types of fuel from oxidation.

REACH: 1907/2006/EC registered; DUIN, KKDIK, K-REACH pre-registered.

CAS: # 128-37-0

Empiric formula: C15H24O

Information provided by JSC, Synthez-Kauchuk

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Ash <= 0.0080 %
Storage Temperature <= 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 69.8 °CEnd
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Appearancewhite crystalline powder without foreign impurities
Color<25APHA
Content<0.2%Other alkyl phenols
 >99.8%Main substance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJSC004 / 317824

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.