MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Resinlab® EP1026 Clear Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Resinlab™ EP1026 Clear is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in viscosity. It gives good resistance to water, salt spray, inorganic acids and bases, and most organic solvents. It was especially formulated to a 1:1 mix ratio for use in either MMD equipment or side-by-side dual cartridges for easy dispensing. A handling cure is normally achieved at room temperature within 20-30 minutes with full cure in 24 hours. An elevated temperature cure schedule can be used to reach final properties quickly.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccPart B; TM R050-16
 1.14 g/ccMixed; TM R050-16
 1.16 g/ccPart A; TM R050-16
Water Absorption 1.56 %
@Time 86400 sec
TM R050-35
Viscosity 15000 cPPart B, RVT, #7, 2.5 rpm; TM R050-12
 15500 cPMixed; TM R050-12
 16000 cPPart A, RVT, #6, 2.5 rpm; TM R050-12
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85TM R050-17
Tensile Strength at Break 6500 psiTM R050-36
Tensile Strength, Ultimate 7500 psiTM R050-36
Tensile Strength, Yield 4000 psiTM R050-36
Elongation at Break 10 - 20 %TM R050-36
Tensile Modulus 450 ksiTM R050-36
Compressive Yield Strength 4000 psiTM R050-38
Compressive Strength >= 28000 psiUltimate; TM R050-38
 >= 28000 psiBreak; TM R050-38
Compressive Modulus 200 ksiTM R050-38
Adhesive Bond Strength 2500 psiLap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 8.00e+14 ohm-cm
Dielectric Constant 4.5
@Frequency 100 Hz,
Temperature 25.0 °C
Dielectric Strength 410 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°C
@Temperature <=34.0 °C
below Tg
 209 µm/m-°C
@Temperature >=34.0 °C
above Tg
Thermal Conductivity 0.185 W/m-K
Maximum Service Temperature, Air 90.0 °C
Minimum Service Temperature, Air -40.0 °C
Glass Transition Temp, Tg 34.0 °CTM R050-25
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %clear; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Pot Life 3.0 - 5.0 minMass: 25g; TM R050-19
 
Descriptive Properties
ColorClear
Mix Ratio1:1Weight and Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 972-1 Thermally Conductive Flexible Epoxy Adhesive
Resinlab® EP950G Gray Aluminum Filled Rubber Modified Epoxy
Resinlab® EP1238 Black Acrylic / Epoxy Hybrid Adhesive
Resinlab® EP1238 Acrylic / Epoxy Hybrid Adhesive
Resinlab® EP11HTFS Gray Filled Epoxy Adhesive

PRESL090 / 101504

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.