MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PPH 3860X Polypropylene, Extrusion Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: High flow reactor grade homopolymer for nonwoven fibers

High Purity - FINA 3860X features extremely high purity for processing in micro denier fibers.

FDA - FINA 3860X complies with all applicable FDA regulations for food contact applications.

Recommended Applications - FINA 3860X is recommended for nonwoven fiber applications.

Processing - FINA 3860X resin processes on conventional extrusion equipment with typical melt temperatures of 450-550°F (232-288°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D1505
Melt Flow 100 g/10 min100 g/10 minASTM D1238L
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 1.655 GPa240.0 ksiASTM D638
Flexural Modulus 1.517 GPa220.0 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Melting Point 165 °C329 °FDSC
 
Processing PropertiesMetricEnglishComments
Melt Temperature 232 - 288 °C450 - 550 °FExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPR 8473 Polypropylene, Film Extrusion Grade
Total 3868 Polypropylene, Extrusion Grade
Total PPR 7450HC Polypropylene, Film Extrusion Grade
Total PPR 7525MZ Polypropylene, Injection Molding Grade
Total PPR 8573 Polypropylene, Film Extrusion Grade

PFIN75 / 38405

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.