MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ashley Polymers Ashlene® 746 Nylon 6/69
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/69

Material Notes: A special copolymer ideal for blown and cast film coextrusion. This is a gel free resin with outstanding lot to lot consistency being produced by a continuous process. It has a lower melting point and is less crystalline than standard Nylon 6.

Data provided by the manufacturer

Key Words: Polyamide 6/69; Ashley Polymers, Inc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccASTM D792
Oxygen Transmission 1.50 cc-mm/m²-24hr-atmcc-mm/m²-24hr-atm. Based on 1 mil microfilm; ASTM D398555-81
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 60.0 MPaATSM D638
Tensile Strength, Yield 26.0 MPaASTM D638
Elongation at Break 362 %ASTM D638
Tensile Modulus 0.335 GPaASTM D638
 
Thermal PropertiesOriginal ValueComments
Melting Point 196 °CASTM D3418

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ashley Polymers Ashlene® 525LD-13G Nylon 66, 13% Glass Reinforced
Ashley Polymers Ashlene® 527LD-14G Nylon 66, 14% Glass Reinforced
Ashley Polymers Ashlene® 742L-13G Nylon 6/66, 13% Glass Reinforced
Plastcom SLOVAMID 6 NG GF 15 HI PA6, 15% glass fibre, improved strength
Polyram PlusTek PA840G13 Nylon 66 for Injection Molding, 13% Glass Fiber Reinforced, Impact Modified, Heat Resistant

PNAA64 / 54411

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.