MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical TR-558A ABS, Transparent, High Strength  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electronic parts, OA machines, toys and others that require transparency and high impact strength. An Izod impact strength or falling dart impact strength of LG transparent ABS is relatively similar to that of general ABS, it is not easily cracked like SAN or PMMA resin in the condition of low impact energy. TR-558 series is good for applications requiring high stiffness.

Since LG transparent ABS TR-558A has excellent transparency and property balance, it could easily be applied on the following products:

    Electric and electronic: Vacuum cleaner parts, air-conditioner panel, humidifier water tank, mixer housing, copier parts, telephone parts, computer housing, facsimile parts, printer panel, washing machine panel and cover, electric fan stand, TV front frame, windows of microwave ovens, calculators, semiconductor carrier box

    Other Applications: Compact cases, cosmetic parts, tool handles, toys, stationeries, game machine

Information Provided by LG Chem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ASTM D792
Melt Index of Compound 24 g/10 min
@Load 10.0 kg,
Temperature 220 °C
24 g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 114114ASTM D785
Tensile Strength, Yield 50.0 MPa7250 psi50 mm/min; ASTM D638
Elongation at Break 35 %35 %50 mm/min; ASTM D638
Flexural Yield Strength 81.4 MPa11800 psi15 mm/min; ASTM D790
Flexural Modulus 2.45 GPa355 ksi15 mm/min; ASTM D790
Izod Impact Notched  2.98 J
@Thickness 3.20 mm
2.20 ft-lb
@Thickness 0.126 in
ASTM D256
 3.24 J
@Thickness 6.40 mm
2.39 ft-lb
@Thickness 0.252 in
ASTM D256
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %2.0 %ASTM D1003
Transmission, Visible 88 %88 %ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 240 °C410 - 464 °F
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature 75.0 - 85.0 °C167 - 185 °F
Dry Time 2 - 4 hour2 - 4 hourPredrying

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical TR-558AI Transparent ABS, High Stiffness, Ice Colored Pellets
Ineos ABS Lustran® 266 ABS, Transparent Grade
LG Chemical AT-553 Transparent ABS, Permanent Antistatic, Natural and Colored Pellets
LG Chemical TR551 MABS, High Transparency, High Rigidity, High Hardness
LG Chemical TR-558 Transparent ABS, Humidity Resistance, Natural and Colored Pellets

PLGCHEM195 / 51016

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.