MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Westlake Epolene® E-14E Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: The Epolene E-14E is a low molecular weight, low density, oxidized polyethylene. The low molecular weight and low softening point contribute to the production of stable, low color emulsions by both atmospheric (wax-to-water) and pressure emulsification methods. Epolene E-14E imparts excellent slip resistance to floor polish films.
    Key Attributes:
  • Imparts slip resistance, durability, and toughness to floor finishes
  • Low density polyethylene (PE)
  • Oxidized to provide functionality
  • Produces stable water based emulsions
    Application/Uses:
  • Automotive refinish
  • Automotive
  • Building and Construction
  • Hot Melt Adhesives
  • Pressure Sensitive Adhesives
  • Solventborne Adhesives
  • Waterborne Adhesives
  • Wax Modification

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.930 - 0.960 g/cc
Viscosity 150 - 300 cP
@Temperature 125 °C
TXAL-A-XX-G-V-005
Brookfield Viscosity 225 cP
@Temperature 125 °C
Molecular Weight 3600 g/mol
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 17
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 204 °C
Ring & Ball Softening Point 104 °CASTM E28
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 3.0TXAL-A-XX-G-VCC-99
 
Descriptive Properties
Penetration Hardness4 dmmASTM D5, Needle under 100-g load for 5s @ 25 deg C, tenths of mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake Epolene® C-26 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed
Westlake Epolene® E-20 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Westlake Epolene® C-19 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed
Westlake Epolene® EE-2 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Westlake Epolene® C-18 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed, Chemically Modified

PWESF9037 / 106874

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.