MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Stanelco Bioplast® GF 106 Biodegradable Plastic
Categories: Polymer; Film; Renewable/Recycled Polymer; Thermoplastic

Material Notes: Bioplast 106 is a versatile soft product, suitable for blown film extrusion of completely biodegradable products. Many customers find it is a natural replacement for LDPE. Made from potato starch mixed with other proprietary brand products for superior flexibility - it is a plasticiser and GM free material.

Bioplast 106 polymer is certified EN 13432 and DIN CERTCO biodegradable and compostable – depending on thickness. Bioplast 106 has EU & FDA (USA) Food Contact Approval for all non high-acidic foods.

This product is also printable by flexographic or offset printing without any pre-treatment and can be coloured with masterbatches.

Bioplast 106 was developed for the packaging, consumer and industrial sectors. Applications include formed parts and film usage, i.e. disposable fast food packaging, carrier bags and refuse sacks.

The product is versatile and can be blown into thin sheet or film applications, injection moulding into virtually any shape and is suitable for blending with Bioplast 2189 in order to create differing properties for specific applications.Bioplast 106 has the ability to ‘drop into’ most applications with little adjustment or affect on performance.

Information provided by Stanelco.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.740 - 0.800 g/ccDIN 53466
Density 1.20 - 1.30 g/ccDIN 53479/A
Melt Density 1.10 - 1.30 g/ccDIN 53735
Particle Size 1500 - 2500 µmDiameter per caliper rule
Moisture Vapor Transmission 3.42 - 4.18 cc-mm/m²-24hr-atm38 µm film; DIN 53122 Part 1
Thickness >= 10.0 micronsDIN 53353
Melt Flow 1.0 - 6.0 g/10 min
@Load 5.00 kg,
Temperature 190 °C
DIN 53735
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 500 - 900 %DIN 53455
Film Elongation at Break, TD 500 - 900 %DIN 53455
Film Tensile Strength at Break, MD 20.0 - 35.0 MPa50% RH; DIN 53455
Film Tensile Strength at Break, TD 20.0 - 35.0 MPa50% RH; DIN 53455
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 65.0 °CVST A/50; DIN 53460
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.50 %BIOTEC Test
Shelf Life 6.00 Monthwith proper storage

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin
EVALCA EVAL® G156A Ethylene Vinyl Alcohol Copolymer Resin
Stanelco Bioplast® GS 2189 Biodegradable Plastic
SK Chemicals SKYTHANE® SG100 SKYGREEN Biodegradable Thermoplastic
FKuR Kunststoff Biograde® C 6509 CL Biodegradable Plastic Compound

PSTAN01 / 79737

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.