MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
ASI® RP5 Cyanoacrylate Super Glue
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: Medium setting: general purpose adhesive designed to bond a wide variety of similar or dissimilar materials. The product is a versatile adhesive offering good climatic, thermal and impact resistance. Its elasticity makes it ideal for bonding dissimilar materials. Handling strength in 5 to 10 seconds. RP 5 has a viscosity of 5 cps and is capable of filling gaps up to .002

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/cc
Viscosity 5.0 cP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 3000 psivs. Grit Blasted Steel; ASTM D2095
Adhesive Bond Strength 160 psiShear vs. Phenolic. Substrate failure.; ASTM D1002
 >= 640 psiShear vs. PVC. Substrate failure.; ASTM D1002
 >= 825 psiShear vs. Polycarbonate. Substrate failure.; ASTM D1002
 >= 885 psiShear vs. ABS. Substrate failure.; ASTM D1002
 >= 1600 psiShear vs. Neoprene rubber. Substrate failure.; ASTM D1002
 >= 1600 psiShear vs. Nitrile rubber. Substrate failure.; ASTM D1002
 2700 - 4300 psi
 3770 psiShear vs. Grit Blasted Steel; ASTM D1002
 3770 psiShear vs. Etched Aluminum; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °F
Minimum Service Temperature, Air -65.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 secFull cure 8 hours
 
Descriptive Properties
BaseEthyl
Color / appearanceclear
MIL A 46050Type II, Class I
SolventRemove Debonder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Valley Adhesives EM-422 High Temperature Application Glue Stick
Toagosei America Aron Alpha® Industrial Krazy Glue™ 803 Cyanoacrylate Adhesive
Parson Adhesives PARLITE® 4760 UV Glue and UV Adhesive for Electronic Assembly
Chemical Concepts H2O Glue® Aquabonder Underwater Adhesive
Bostik 6332 Quick Setup EVA Glue Stick

PASINC9001 / 233368

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.