MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Visico™ LE4421/LE4432 Polyolefin/Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Polyolefin

Material Notes: Visico LE4421/LE4432 is a silane crosslinkable black compound system designed for insulation of low voltage energy cables and covering/insulation of overhead cables. Visico LE4421 is a low density polyethylene, copolymerized with vinyl silane. LE4432 is a crosslinking catalyst masterbatch specially designed to be used with Visico base resins. The system crosslinks quickly in sauna or in hot water. Cable insulation with a proper mixture of Visico LE4421 (90 parts) and LE4432 (10 parts) exhibits excellent thermo-oxidative stability. The combination is suitable for both copper and aluminum conductors. The final product contains nominal 2,5% of fine size carbon black ensuring excellent weatherability.

Applications: Visico LE4421/LE4432 is designed for: Covering/insulation of overhead cables; Insulation of low voltage energy cables, range up to 6 kV

Specifications: Visico LE4421/LE4432 in combination meets the applicable requirements as below when processed using sound extrusion and testing procedure: IEC 60502-1; ICEA S-105; Canadian Standards Association C22.2 No. 38 Cable Type RW-90 Outdoor; ANSI/ICEA S-70-547

Special Features: Visico LE4421/LE4432 insulation system offers:

  • Excellent processing properties
  • Low scorch allowing long runs and more frequent tooling changes
  • Excellent surface finish
  • Less smell, more consistent quality (no volatiles)
  • Good curing speed
  • No drying prior to extrusion
  • Excellent storage stability

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.923 g/ccBase Resin; ISO 1183-1, Method A
 1.04 g/ccMasterbatch; ASTM D 792
Melt Flow 1.00 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
Storage Temperature 10.0 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50.0
@Time 1.00 sec
ISO 868
Tensile Strength >= 15.0 MPa250 mm/min; IEC 60811-501
 >= 121 MPa
@Treatment Temp. 135 °C,
Time 605000 sec
After ageing; IEC 60811-401
Elongation at Break 0.000 %ICEA T-28-562
 60.0 %ICEA T-28-562
 >= 200 %250 mm/min; IEC 60811-501
 >= 240 %
@Treatment Temp. 121 °C,
Time 605000 sec
After Ageing; IEC 60811-401
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 10.0 ohm-cm[POcm]; IEC 60093
Dielectric Constant <= 2.50
@Frequency 60 Hz
ASTM D150
Dielectric Strength >= 20.0 kV/mmIEC 60243
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= 0.760 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Zone 1 145 °C
Zone 2 165 °C
Zone 3 170 °C
Zone 4 170 °C
Die Temperature 175 °C
Melt Temperature <= 200 °C
Shelf Life 18.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9929 / 323286

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.