MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dioshy MP-885 SBS
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Features:
  • Non-hydrogenated grades; silicone and rubber touch; broad hardness range (Shore A 0 ~ Shore D 45).
  • Suitable to mostly products; economic efficiency; good adhesion properties.
  • Excellent anti-slip and good tensile strength; transparent or white color, good coloring ability; customized.
  • Suitable to dual color processing for PP, PE or PS; also can be the toughener for PP, PE or PS.
  • Suitable to mostly thermoplastic procedures; PVC replacement.
  • Green material, passed heavy metal regulation, RoHS and EACH –SVHC .

Information provided by DIOSHY CO., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.007 g/ccJIS-K6301
Melt Flow 22.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
JIS-K7210
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85JIS-K6301
Hardness, Shore D 35JIS-K6301
Tensile Strength 39.0 kg(f)/cm²JIS-K6310
Elongation at Break 312 %JIS-K6310
100% Modulus 31.0 kg(f)/cm²JIS-K6310
300% Modulus 13.0 kg(f)/cm²JIS-K6310
Tear Strength 328 kg(f)/cmJIS-K6310-B
Compression Set 32 %
@Temperature 23.0 °C,
Time 79200 sec
JIS-K6301
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 160 - 175 °CInjection
 165 - 175 °CExtrusion
Middle Barrel Temperature 175 - 185 °CInjection
 180 - 195 °CExtrusion
Front Barrel Temperature 180 - 195 °CExtrusion
 185 - 195 °CInjection
Nozzle Temperature 195 - 205 °CInjection
Die Temperature 190 - 205 °CExtrusion
Drying Temperature 80.0 °C
Dry Time 1.00 hour
 
Descriptive Properties
Application Dual color processingPP
ColorWhite
TPS typeSBS

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDIOSH007 / 294617

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.