MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Fused Quartz
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Silicon dioxide.

Information below is typical for commercially available fused quartz used for tubing and lighting applications. A wide variation of properties is possible between specific grades.

Key Words: SiO2, Silica, Silicon Dioxide
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.20 g/cc
Water Absorption 0.00 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 820
Hardness, Mohs 5.5 - 7.0
Modulus of Elasticity 70.0 - 78.0 GPa
Compressive Strength 1100 MPa
Poissons Ratio 0.17
Shear Modulus 31.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 - 1.00e+22 ohm-cm
Dielectric Constant 3.7 - 6.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.400 µm/m-°C
@Temperature 20.0 °C
 0.450 µm/m-°C
@Temperature 1000 °C
 0.600 µm/m-°C
@Temperature 500 °C
 0.700 µm/m-°C
@Temperature 250 °C
Specific Heat Capacity 0.700 J/g-°C
 0.670 - 0.750 J/g-°C
Thermal Conductivity 1.40 - 2.00 W/m-K
Softening Point 1580 - 1730 °C
Annealing Point 1100 - 1215 °C
Strain Point 990 - 1120 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.46
Transmission, Visible >= 90 %
 
Descriptive Properties
ColorClear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quartz (SiO2)
Silicon Dioxide, SiO2 (Alpha Quartz)
96% Silica Consolidated Reconstructed Glass
Borosilicate Glass
Borosilicate Glass, Low Expansion

BQUARTZ / 288

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.