MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röhm Plexiglas® GS 249 Cast Acrylic  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Cast

Material Notes: Description: PLEXIGLAS® GS 249 is another cast acrylic specially developed to meet even higher demands by the aviation industry, but is additionally crosslinked. As compared with uncrosslinked acrylic, it offers higher resistance to media that cause stress cracking and increased heat distortion resistance. PLEXIGLAS® GS 249 is also excellently suited for stretching, which makes it possible to improve its properties even further over the unstretched state. Typical applications are cabin windows in civilian aircraft, glazing for pressurized aircraft cabins, cockpit glazing, canopies and windshields.

Information provided by degussa.

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183, ASTM D792
Water Absorption 0.20 %MIL-P-8184
Water Absorption at Saturation 2.1 %MIL-P-8184
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPaISO 527-2/1B/5, ASTM D638
Elongation at Break 5.0 %ISO 527-2/1B/5, ASTM D 638
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
EN 2155-12, ASTM D696
Maximum Service Temperature, Air 113 °CISO 71-2Ae, ASTM D648
Vicat Softening Point 118 °CISO 306-B-50
Flame Spread 0.600 in/minFire Rating; ASTM D635
 20.0 mm/minFire Rating; EN 3844-2
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49ISO 489, ASTM D542
Haze 1.5 %Original State; EN 2155-9, ASTM D1003
 2.2 %after artificial weathering; EN 2155-9, ASTM D1003
Transmission, Visible 89 %after artificial weathering; ASTM D1003
 91 %Original State; EN 2155-5, ASTM D1003
UV Transmittance <= 1.0 %
@Wavelength 290 - 330 nm
 
Descriptive Properties
Angular DeviationMax 4 minutesEN 2155-7 (ASTM D637)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm Plexiglas® GS 245 Cast Acrylic
Overview of materials for Acrylic, Cast
Lucite International Perspex™ GS Acrylic Cast Sheet 000/0000
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade
Röhm Plexiglas® GS 0F00 (233) Cast Acrylic

PHUK032 / 47166

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.