MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPH 3860X Polypropylene Homopolymer, High Flow Reactor Grade for Non-Woven Fibers
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Fiber Grade

Material Notes: High Purity TOTAL Petrochemicals Polypropylene 3860X features extremely high purity for processing in micro denier fibers.

Recommended Applications. 3860X is recommended for nonwoven fiber applications.

FDA. 3860X complies with all applicable FDA regulations for food contact applications.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.905 g/ccASTM D1505
Melt Flow 100 g/10 minASTM D1238, L
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 1655 MPaASTM D638
Flexural Modulus 1517 MPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 3860X Polypropylene, Extrusion Grade
Total PPH 3962 Polypropylene Homopolymer, Ultra-High Melt Flow Rate Pelletized For Melt Blown Fiber Applications
Total PPH 3862 Homopolymer Polypropylene, Fiber Grade
Total 3861 Polypropylene, Extrusion Grade
Total PPR 6827MZ Polypropylene, Random Copolymer - High Flow Clarified - for Injection Molding

PTOTAL809 / 130534

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.