MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Nouryon Trigonox 101-7.5PP 2,5-Dimethyl-2,5-di(tert-butylperoxy)hexane, 7.5% on polypropylene carrier
Categories: Other Engineering Material

Material Notes: Trigonox 101-7.5PP is a peroxide formulation for the production of controlled rheology polypropylene (CRPP).

CAS number: 78-63-7

EINECS/ELINCS No: 201-128-1

Applications: Controlled rheology polypropylene: Trigonox 101-7.5PP is an efficient peroxide formulation for the controlled rheology of polypropylene (CR-PP) in the temperature range of 200-250°C. This powder form masterbatch of the liquid Trigonox 101-7.5PP allows a more accurate dosage of the peroxide to the polymer. Also a more homogeneous distribution of the peroxide throughout the polymer is of advantage. Using the powder form formulation rather than the liquid form results in a better control of the visbreaking process. Trigonox 101-7.5PP allows polypropylene producers great flexibility in controlling a polymer's Melt Flow Index (MFI). Small changes in either peroxide concentration or process temperature can produce significantly different MFI's.

Information provided by Nouryon

Vendors:
Available Properties
  • Bulk Density
  • Half-life, [hr]
  • Half-life, [hr]
  • Half-life, [hr]
  • Molecular Weight
  • Storage Temperature
  • Decomposition Temperature, Self-Accelerating Decomposition Temperature
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.