MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Copper Casting Alloy, UNS C87500, M05 Temper, As Permanent Mold Cast
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: As Permanent Mold Cast

Casting Characteristics: High – Fluidity; Medium – Shrinkage in Solidification, Casting Yield, Effect of Section Size, Gassing; Low –Drossing

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Gas Shielded Arc Welding; Good Suitability - Spot Weld, Seam Weld, Butt Weld; Fair Suitability – Oxyacetylene Welding

Typical uses: Window Hardware; Bearings; Fittings; Gears; Impellers; Levers; Pump Fixtures; Valve Bodies; Boat Parts; Small Boat Propellers; Fixtures

Applicable Specifications: As Centrifugal Cast - Castings SAE J462, Castings SAE J461, Castings ASTM B271/B271M; As Permanent Mold Cast - Castings ASTM B806; As Sand Cast – Castings ASTM B584, Castings ASTM B763/B763M; Ingot - ASTM B30

Vendors:
Available Properties
  • Density
  • Tensile Strength, for Standard
  • Tensile Strength, Yield, for Standard, 0.5% Ext
  • Elongation at Break, for Standard
  • Tensile Modulus
  • Machinability
  • Electrical Resistivity, 6.7% IACS
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Shrinkage, Patternmaker's Shrinkage (3/16 in./ft.)
  • Processing Temperature, Stress Relief
  • Aluminum, Al
  • Copper, Cu
  • Lead, Pb
  • Silicon, Si
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.