MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 185,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Abatron AboWeld 48-8/AboCure 48-8 Adhesive/Casting Resin
Categories: Polymer; Adhesive; Thermoset

Material Notes: Information provided by Abatron, Inc. Adheres to metal, glass, ceramics, wood, masonry, etc. Material properties are based on a 2/1 mix ratio. Resin is white, curing agent is black. Gray blend allows for visual inspection of proper mixing and ratios. Shelf life: 12+ months (unmixed).

Processing:100/(40-100) ratio. Pot life: 100 g, 30-40 min. at 25°C(77°F). Hardens in 3-5 hours at 25°C (77°F), 4-6 min. at 80°C (175°F), 2 min. at 120°C (250°F), 24 sec to 1 min. at 150°C (300°F).

Corrosion Resistance: good resistance to atmospheric conditions, soft and salt water, alkalis and diluted acids.

Key Words: potting, casting, encapsulating, impregnating
Vendors:
Available Properties
  • Water Absorption, after 24 hrs.
  • Viscosity Measurement
  • Hardness, Shore D, 100/40 pbw; 68 at 100/80 pbw; 66 (60 after 10 sec) at 100/100 pbw
  • Tensile Strength, Ultimate, Typical averaged test results for Abatron Adhesive/Casting Resins.
  • Elongation at Break, Typical for Abatron Adhesive/Casting Resins.
  • Flexural Yield Strength, Typical averaged test results for Abatron Adhesive/Casting Resins.
  • Compressive Yield Strength, Typical averaged test results for Abatron Adhesive/Casting Resins.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.