MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.
Master Bond EP21AOLV-2MED Two Component Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Key Features:
  • Excellent thermal conductivity
  • Room temperature curing
  • Convenient one to one mix ratio
  • Superior electrical insulation
  • Meets USP Class VI requirements
  • Passes ISO 10993-5 tests for cytotoxicity
Product Description: Master Bond EP21AOLV 2Med is a two component, thermally conductive, electrically isolating epoxy adhesive, sealant, coating and encapsulant. It has a convenient, one to one mix ratio by weight, a smooth consistency and good flow properties. EP21AOLV-2Med cures readily at room temperature and can be accelerated by heat. The optimum cure schedule is overnight at room temperature followed by 2-4 hours at 150-200°F. Most importantly, it has been rigorously tested for biocompatibility and passes USP Class VI testing as well as ISO 10993-5 for cytotoxicity. Its viscosity and flow properties enable it to be used for bonding as well as potting. It bonds well to a wide variety of substrates including metals, composites, glass, ceramics, plastics and many rubbers. This system resists many chemicals including water, oils, fuels and most notably, EtO, radiation and many cold sterilants. EP21AOLV-2Med has a wide array of desirable physical strength properties including superb dimensional stability, a high modulus, exceptional compressive strength and very low shrinkage upon curing. It should be emphasized that this system is a fine thermal conductor while retaining impressive electrical insulation properties. Its service temperature range is -60°F to +250°F. The color of Part A is gray; the color of Part B is off-white. It’s widely used in the medical device industry and other applications where biocompatibility, thermal conductivity and electrical insulation are essential requirements.

Product Advantages:

  • Convenient handling, easy to use, one to one mix ratio by weight
  • Smooth, flowable consistency. Ideal for bonding and potting
  • Adheres well to many different substrates
  • Desirable physical strength properties, low coefficient of thermal expansion
  • Combines outstanding thermal conductivity and laudable electrical insulation properties
  • Stellar resistance to chemical sterilants, radiation and EtO
  • Passes USP Class VI biocompatibility testing and ISO 10993-5 cytotoxicity requirements

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part A
  • Viscosity, Part B, thixotropic
  • Hardness, Shore D
  • Tensile Strength
  • Tensile Modulus
  • Compressive Strength
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, in original, unopened containers
  • USP Class VI
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

USP Class VI adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.