MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Greene Tweed CHEMRAZ® 615 Perfluoroelastomer
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: Greene Tweed’s Chemraz® 615 exhibits outstanding high temperature properties, with a temperature range from 0°F to 615°F (-18°C to 324°C). Chemraz 615’s chemical resistance and low compression set characteristics combine to outperform tin-cured perfluoroelastomers.

Chemraz 615 shows lower compression set at high temperatures and higher retained sealing force than other perfluoroelastomers available.

Because Chemraz 615 allows for the use of higher process operating temperatures, it is ideal for a range of markets, from chemical process to petroleum refining. This superior perfluoroelastomer performs well in a variety of fluids such as inorganic and organic chemicals, acids, reagents, heat transfer fluids and hydrocarbons.

Chemraz 615 is available in standard O-rings and custom shapes for a range of equipment, from pumps and valves to agitators and mixers, from mechanical seals and process control instruments to heat exchangers and diagnostic equipment.

Applications:

  • Mechanical seals
  • Process control instruments
  • Heat exchangers
  • Valves
  • Agitators & mixers
  • Pumps
  • Couplings

Information provided by Greene Tweed.

Vendors:
Available Properties
  • Specific Gravity, ASTM D297
  • Hardness, Shore A, ASTM D2240
  • Tensile Strength at Break, ASTM D1414
  • Tensile Strength, Yield, ASTM D1414, @50% Elongation
  • Tensile Strength, Yield, ASTM D1414, @100% Elongation
  • Elongation at Break, ASTM D1414
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.