Polyamide PA66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. Technyl A 218 V30 is used in all sectors of industry, offering an excellent combination between thermal and mechanical properties. This grade is commonly used in the automotive industry for engine components, such as water tanks, degassing and liquid containers, engine covers, and various housing. This product is available in natural, black and in colors on request. Glow wire test thick. 1,6 mm, IEC 695-2-1, is 700°C. Information provided by Rhodia; Rhodia has been acquired by Solvay. DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe. |