MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Poco Graphite Premium Graphite Industrial Graphite Grade AXF-5QC
Categories: Carbon; Graphite

Material Notes: AXF-5QC graphite is impregnated with copper to reduce resistivity and friction, and increase lifetime of the products this material is machined into. Impregnating AXF-5Q graphite with copper greatly increases the material's compressive strength and reduces its electrical resistivity and friction coefficient at operating temperatures below 300°C. Features: Average particle size of less than 5 microns provides high strength and resistance to damage. Copper impregnation increases product lifetime reduces replacement needs. Fine surface finish creates parts with precision details. Low friction coefficient is ideal for sliding friction or high-load applications at relatively low temperatures. We can enhance this material with our post-processing options. Our graphite grades are available as semi-finished rods, blocks, plates, and fully machined parts. Applications: Air bearings. Aerospace. Satellite optics. Hot press dies. Furnace components. Crucible materials.

Information provided by Entegris POCO Materials.

Vendors:
Available Properties
  • Density
  • Particle Size
  • Flexural Strength
  • Compressive Strength
  • Electrical Resistivity
  • CTE, linear
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Poco Graphite - Entegris

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.