MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Trinseo Magnum™ 2642 ABS, Impact Grade  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded

Material Notes: MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.

The 2600 series of MAGNUM ABS resins are designated for use in healthcare applications. Both high and low gloss resins are available which have passed the USP XXIII Class IV medical testing. Other non-USP classified testing is also done on the MAGNUM 2600 series of ABS resins to evaluate the biocompatibility of the resins.

MAGNUM 2642 ABS resin is a low gloss ABS with impact resistance and processability similar to the high gloss MAGNUM 2610 ABS resin. With a melt flow rate of 6 g/10 min. and an Izod impact strength of 160 J/m, MAGNUM 2642 is suitable for many healthcare applications.

Data provided by Dow Chemical.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors:
Available Properties
  • Density, ASTM Data
  • Linear Mold Shrinkage
  • Melt Flow, ASTM Data
  • Hardness, Rockwell R
  • Tensile Strength, Yield, ASTM Data
  • Elongation at Yield, ISO Data
  • Tensile Modulus, ASTM Data
  • Izod Impact, Notched, ASTM Data
  • Charpy Impact Unnotched, ISO Data, Low Temp
  • Charpy Impact Unnotched, ISO Data
  • Charpy Impact, Notched, ISO Data, Low Temp
  • Charpy Impact, Notched, ISO Data
  • Instrumented Impact Total Energy
  • CTE, linear, Parallel to Flow, ISO data
  • Deflection Temperature at 0.46 MPa (66 psi), Unannealed; ASTM Data
  • Deflection Temperature at 1.8 MPa (264 psi), Unannealed; ASTM Data
  • Deflection Temperature at 1.8 MPa (264 psi), Annealed; ASTM Data
  • Vicat Softening Point
  • Gloss, Gardner Gloss, 60°
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Trinseo, former Styron

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.