| Molecular Formula: C30H17Cl IUPAC Name: 1-chloro-9,10-bis(2-phenylethynyl)anthracene Synonyms: 1-CHLORO-9,10-BIS(PHENYLETHYNYL)ANTHRACENE;1-CHLORO-BPEA;CBPEA;1-chloro-9,10-bis(phenylethynyl)-anthracen;1-CHLORO-9,10-BIS(PHENYLETHYNYL)ANTHRACENE 96+%;9,10-Bis(phenylethynl)-1-chloroanthracene;1-Chloro-9,10-bis(phenylethynyl)anthracene,97%;1-Chloro-9,1 SMILES: C1=CC=C(C=C1)C#CC2=C3C=CC=C(C3=C(C4=CC=CC=C42)C#CC5=CC=CC=C5)Cl InChI=1S/C30H17Cl/c31-29-17-9-16-27-26(20-18-22-10-3-1-4-11-22)24-14-7-8-15-25(24)28(30(27)29)21-19-23-12-5-2-6-13-23/h1-17H; InChiKey = IMMCAKJISYGPDQ-UHFFFAOYSA-N Alfa Chemistry Materials product group: Semiconductor Manufacturer data sheet |