MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Wacker Silres® Powder D Silicone Masonry Water Repellent
Categories: Polymer; Thermoset; Silicone

Material Notes: Product description: SILRES® Powder D is a water-redispersible silicone water-repellent in powder form and used as a highly efficient additive. SILRES® Powder D acts as outstanding water repellent even at very low concentrations without affecting the water vapour permeability.SILRES® Powder D contains a fine mineral filler as antiblocking agent.

Special features:

  • redispersible technology i.e. excellent mixability with water
  • based on highly efficient silicones
  • solventless
Application: SILRES® Powder D is a high-quality specialty product for enhancing the water repellency and water resistance of non load-bearing precast concrete products or mineral construction material mixes, e.g. premixed plasters, joint mortars and powder paints. Properly formulated products exhibit:
  • low water absorption coefficients
  • excellent droplet effect
  • low soiling tendency
  • durability
SILRES® Powder D can be used in both dry powder and liquid systems.

Information provided by Wacker Chemie AG.

Vendors:
Available Properties
  • Bulk Density
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.