MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Morgan Advanced Ceramics Deranox™ 970 Mac-A970R Aluminum Oxide Ceramic
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: High-quality alumina ceramic of 97.0% Al2O3 content. This material is an excellent electrical insulator that can be metallized to facilitate high-temperature brazing of assemblies.

Prime Features:

  • Readily accepts metallizing with moly-manganese
  • Very high volume resistivity
  • Low loss, constant high dielectric
  • High density, non-porous and vacuum tight
  • Resists abrasive wear and chemical attack
Typical Applications: Metallized ceramic components used in high-integrity applications, including:
  • High-vacuum systems
  • Laser equipment (gas, solid-state and waveguide)
  • X-ray tubes and electron microscopes
  • Microwave windows
  • Insulators in medical and scientific equipment
Production Capabilities:
  • Complex pressed and machined components
  • Grinding, lapping polishing to precise limits
  • Moly-manganese metallizing
  • Brazed assemblies

Information provided by Morgan Advanced Materials

Key Words: Mac-A970R
Vendors:
Available Properties
  • Density, fired
  • Open Porosity, fully dense, % nominal, apparent
  • Grain Size
  • Hardness, Vickers, [GPa]
  • Modulus of Elasticity, Young's
  • Flexural Strength, 3-point
  • Compressive Strength
  • Fracture Toughness
  • Volume Resistivity
  • Volume Resistivity
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor, tan d
  • Dissipation Factor, tan d
  • Dissipation Factor, tan d
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Maximum Service Temperature, Air, no load
  • Al2O3
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.