MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
LyondellBasell Adflex KS 311 P Thermoplastic Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Adflex KS 311 P is a reactor TPO (thermoplastic polyolefin) manufactured using Lyondell Basell's proprietary Catalloy process technology. It is suitable for extrusion as well as injection molding and blow molding applications, including mechanical and decorative automotive parts requiring elastomeric type properties, like molded-in color automotive exterior components. The product is used by our customers for applications with paintable and weatherable requirements, such as injection molded fascias, claddings, bumper covers, body panels, step pads, and air deflectors. It is also used as a component in compounded materials for a wide range of industrial applications. The grade is available in natural pellet form.

Availability: Africa-Middle East; Asia-Pacific; Australia and New Zealand; North America; South & Central America

Application: Exterior Automotive Applications; Single Ply Roofing; Specialty Film; Stationery Film

Market: Automotive; Compounding; Industrial, Building & Construction

Processing Method: Cast Film; Compounding; Extrusion Blow Molding; Injection Molding

Attribute: Good Colorability; Good Flexibility; Good Moldability; Good Processability; Good Surface Finish; Low Temperature Impact Resistance

Information provided by LyondellBasell.

Vendors:
Available Properties
  • Density, ISO 1183-1, Method A
  • Melt Flow, ISO 1133-1
  • Hardness, Shore D, ISO 868
  • Tensile Strength at Break, ISO 527-1, -2
  • Tensile Strength, Yield, ISO 527-1, -2
  • Elongation at Break, ISO 527-1, -2
  • Elongation at Yield, ISO 527-1, -2
  • Flexural Modulus, ISO 178
  • Charpy Impact, Notched, ISO 179, Complete Break
  • Charpy Impact, Notched, ISO 179, Partial Break
  • Charpy Impact, Notched, ISO 179, Partial Break
  • Impact Test, ASTM D3763, Multi-axial, 6.6 m/s, 3.2 mm plaque, Note: Failure Mode - Ductile
  • Impact Test, ASTM D3763, Multi-axial, 6.6 m/s, 3.2 mm plaque, Note: Failure Mode - Ductile
  • Tear Strength, ASTM D624
  • Melting Point, ISO 11357-3
  • Deflection Temperature at 0.46 MPa (66 psi), ISO 75B-1, -2, Unannealed
  • Vicat Softening Point, ISO 306, A/50
  • Haze, ASTM D1003
  • Gloss, ASTM D2457, 60°
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
LyondellBasell (former Equistar)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.