A nickel-iron-chromium alloy with an addition of silicon. It has good high-temperature strength and excellent resistance to oxidation and carburization. The silicon content makes the alloy resistant to internal oxidation in high-temperature atmospheres that vary between oxidizing and reducing. Used in industrial furnaces and for heat-treating baskets, trays, and fixtures. Standard product forms are round, plate, sheet, strip, tube, pipe, and wire. Data provided by the manufacturer, Special Metals. |