MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
AISI 4340 Steel, oil quenched 830°C (1525°F), 540°C (1000°F) temper, nitrided
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 4000 Series Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: Specimens nitrided at 525°C for 48 hrs. Normalized at 940 - 955°C.

AISI 4340 has a favorable response to heat treatment (usually oil quenching followed by tempering) and exhibits a good combination of ductility and strength when treated thusly. Uses include piston pins, bearings, ordnance, gears, dies, and pressure vessels.

Key Words: alloy steels, UNS G43400, AMS 5331, AMS 6359, AMS 6414, AMS 6415, ASTM A322, ASTM A331, ASTM A505, ASTM A519, ASTM A547, ASTM A646, MIL SPEC MIL-S-16974, B.S. 817 M 40 (UK), SAE J404, SAE J412, SAE J770, DIN 1.6565, JIS SNCM 8, IS 1570 40Ni2Cr1Mo28, IS 1570 40NiCr1Mo15
Vendors:
Available Properties
  • Density
  • Hardness, Knoop, Converted from Rockwell C hardness.
  • Hardness, Rockwell C, core hardness
  • Hardness, Vickers, Converted from Rockwell C hardness.
  • Modulus of Elasticity
  • Bulk Modulus, Estimated from elastic modulus
  • Poissons Ratio, Typical for steel
  • Fatigue Strength, Notched; Nitrided samples have no true limit; R.R. Moore rotating beam fatigue specimens with min. diameter of 5.84 mm; 45°, 0.25 mm root-radius notch 0.51 mm deep.
  • Fatigue Strength, Smooth; Nitrided samples have no true limit; R.R. Moore rotating beam specimens
  • Machinability, annealed and cold drawn. Based on 100% machinability for AISI 1212 steel.
  • Shear Modulus, Estimated from elastic modulus
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • CTE, linear, specimen oil hardened, 600°C (1110°F) temper
  • CTE, linear, 1.88% Ni, normalized and tempered
  • CTE, linear, specimen oil hardened, 600°C (1110°F) temper
  • CTE, linear, specimen oil hardened, 600°C (1110°F) temper
  • CTE, linear, 1.88% Ni, normalized and tempered
  • CTE, linear, 1.90% Ni, quenched, tempered
  • CTE, linear, specimen oil hardened, 600°C (1110°F) temper
  • Specific Heat Capacity, Typical 4000 series steel
  • Thermal Conductivity, Typical steel
  • Carbon, C
  • Chromium, Cr
  • Iron, Fe, As remainder
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.