MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Colmant Coated Fabrics BUTYL (IIR) Coated Polyester Fabric
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Butyl coated polyester fabric combines the following properties: BUTYL rubber is an interesting option for applications in extreme temperatures. It has an excellent behaviour at cold temperatures (up to -60°C). It keeps a good resistance to acids, ketones and oils. Polyester is a synthetic fiber that ranks first in the world in terms of production. It is a linear polymer whose mass includes a majority (80% minimum) of ester functions and terephthalic acid. Polyester yarn is light and flexible. It is resistant to ultraviolet radiation. Polyester fabric is hardly inflammable. It softens around 245°C, and melts around 250°C. It retains a good shape memory and can therefore be used in the composition of crease-resistant fabrics. Moreover, a suitable weave also allows a good evacuation of heat.

Applications:

  • Industrial fabrics
  • straps
  • tarps
  • tires
  • rope
  • clothing
  • Inner tubes
  • tire curing bladder
Properties:
  • Acids resistant
  • Non-skid
  • UV resistance
  • Ozone Resistance

Information provided by COLMANT COATED FABRICS

Vendors:
Available Properties
  • Hardness, Shore A
  • Tensile Strength at Break
  • Elongation at Break
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.