Bapolene LD200F is a general purpose low density polyethylene for blown film extrusion applications. It contains medium levels of slip/antiblock additives. This product meets US FDA 21 CFR 177.1520. Applications: Blown Film; Film; General Purpose clarity applications. Film properties below are based on a thickness of 32 µm and blow-up ratio of 2:1. Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers |
Food Contact Acceptable; General Purpose; Low Density; Medium Antiblocking; Medium Slip |