MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Kohesi Bond KB 1427 HT One component, chemically resistant epoxy for bonding, coating, sealing and casting
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Product Highlights:
  • service up to 340°C
  • Admirable chemical resistance
  • Excellent flow properties
  • Low exotherm upon curing
  • Superior electrical insulation
  • Unlimited working life at room temperature
Kohesi Bond KB 1427 HT is a marvelous single component epoxy system for bonding, coating, sealing and casting applications. Although it requires a minimum temperature of 150°C for curing, it can achieve faster cures at elevated temperatures. KB 1427 HT offers an extremely wide service temperature range of -60°C to +340°C, with a roaring glass transition temperature (Tg) of 220°C - 230°C. This product’s exquisite flow properties and unlikely low exotherm makes it ideal for use in casting well beyond 1/2 inch thicknesses. Being a one component system, it provides ease of application and also adheres well to a wide variety of substrates including metals, ceramics, composites, most plastics and glass. It provides first-rate mechanical strength properties and dimensional stability. In addition to superior electrical insulation, KB 1427 HT also offers excellent chemical resistance to a variety of fuels, oils and water even at higher temperatures. It has a tan color. It is highly recommended to post cure the epoxy at 180°C for 2 - 12 hours in order to achieve optimum properties. Owing to its magnificent performance and ease of use, KB 1427 HT is ideal for use in aerospace, oil and chemical processing, electronics and various OEM applications.

Typical Applications:

  • Bonding
  • Sealing
  • Coating
  • Casting

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors:
Available Properties
  • Viscosity
  • Hardness, Shore D
  • Tensile Modulus
  • Compressive Strength
  • Adhesive Bond Strength, Tensile Lap Shear, Al/Al
  • Adhesive Bond Strength, Tensile Lap Shear, Al/Al
  • Volume Resistivity
  • Dissipation Factor
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Glass Transition Temp, Tg
  • Cure Time, Option 2
  • Cure Time, Option 1
  • Cure Time, Optimum Cure: 150°C for 4 - 6 hours, plus 180°C for 12 - 24 hours
  • Shelf Life, in original unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.