MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Chemically Resistant adhesives
Epoxy Technology EPO-TEK® E2001-HV Electrically Conductive, Silver-Filled Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: Product Description: EPO-TEK® E2001-HV Is a snap cure, two component, silver-filled die attach adhesive for semiconductor plastic IC packaging.

Advantages & Application Notes:

  • Snap cure adhesive or fast-cure; chips can be cured in-line < 90 seconds travel time; or lead-frames can be loaded into magazines for box oven curing <15 minutes travel time at 180°C or higher; a traditional box-oven cure for several hours may also be used.
  • Excellent adhesion to die-paddle on lead-frames including Cu, Alloy 42, or Ag spot ring.
  • Bright and shiny silver epoxy after cure; suggested for LED die-attach packaging.
  • Compatible with COB die-attach process on Au plated PCB, Au plated ceramic PCB in hybrid packages or opto-electronic packaging using hybrids.
  • 24 hour pot-life for automated syringe dispensing; compatible with many dispensing methods: air pressure, positive displacement, and auger screws.
  • Soft and creamy thixotropic behavior. Rheology allows for high speed dispensing of dots, dot arrays, shower head dispensing, or the writing-pen method.
  • Suggested for JEDEC Level II packaging of semiconductor devices

Information Provided by Epoxy Technology

Vendors:
Available Properties
  • Specific Gravity, Part B
  • Specific Gravity, Part A
  • Particle Size
  • Viscosity, 20 rpm
  • Ionic Impurities - Na (Sodium)
  • Ionic Impurities - K (Potassium)
  • Ionic Impurities - Cl (Chloride)
  • Hardness, Shore D
  • Tensile Modulus, Storage
  • Shear Strength, Lap
  • Shear Strength, Die
  • Volume Resistivity
  • CTE, linear, Below Tg
  • CTE, linear, Above Tg
  • Thermal Conductivity
  • Maximum Service Temperature, Air, Continuous
  • Maximum Service Temperature, Air, Intermittent
  • Minimum Service Temperature, Air, Continuous
  • Minimum Service Temperature, Air, Intermittent
  • Glass Transition Temp, Tg, Dynamic Cure 20—200°C /ISO 25 Min; Ramp -10—200°C @ 20°C/Min
  • Decomposition Temperature, TGA, Degradation Temperature
  • Cure Time, Bond Line
  • Cure Time, Bond Line
  • Pot Life
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Chemically Resistant adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.