MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Borealis Himod™ FT3280 LDPE for Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Himod FT3280 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and improved optical properties. Benefits can be obtained in terms of better down gauging possibilities and improved processability. Excellent printing quality is obtained due to high clarity and better layout.

Himod FT3280 is intended for applications like: Stiff, transparent shrink films with high surface gloss and co-extrusion applications.

Information provided by the Manufacturer.

Vendors:
Available Properties
  • Density, ISO 1183
  • Thickness
  • Melt Flow, ISO 1133
  • Film Elongation at Break, MD, ISO 527-3
  • Film Elongation at Break, TD, ISO 527-3
  • Secant Modulus, MD, ASTM D882-A
  • Secant Modulus, TD, ASTM D882-A
  • Impact, ASTM D5748, Puncture Resistance, force (N)
  • Puncture Energy, ASTM D5748
  • Coefficient of Friction, Dynamic, ISO 8295
  • Tear Strength, Total, ISO 6383/2, TD
  • Tear Strength, Total, ISO 6383/2, MD
  • Dart Drop, ISO 7765/1
  • Film Tensile Strength at Break, MD, ISO 527-3
  • Film Tensile Strength at Break, TD, ISO 527-3
  • Melting Point, ISO 11357/03
  • Vicat Softening Point, ISO 306, A (10N)
  • Haze, ASTM D1003
  • Gloss, ASTM D2457
  • Transmission, Visible, transparent; thickness not quantified
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.